STANDARD TEST METHOD |
CONBLOCK CDA RESULTS VS. REFERENCE |
CRD-C48 Permeability of Concrete |
Coefficient of permeability rating (K)=1.2x 1013 (96% reduction, 21 days |
ASTM C39 Compressive Strength of Concrete |
>10% increase after 3 days; >10% increase after 28 days |
ASTM C666 Freeze-Thaw Durability |
Passed 300 cycles |
ASTM C1585 Measurement of Rate of Absorption of Water by Hydraulic Cement Concretes |
36% reduction after 90 days |
ASTM C157 Length Change of Hardened Hydraulic-Cement Mortar and Concrete |
Dry shrinkage of 0.033% (330 microstrain) after 56 days; 23% less than reference |
ASTM C1567 Determining the Potential Alkali-Silica Reactivity of Cementitious Materials and Aggregate |
21% reduction after 28 days |
ASTM C1260 Determining the Potential Alkali-Silica Reactivity of Aggregates |
20% reduction after 28 days |
ASTM C1760 Bulk Electrical Conductivity of Hardened Concrete |
13% reduction at 1000 Hz |
BS EN 12390-8 Depth of Water Penetration under Pressure |
32% reduction after 90 days |